Composition
KRISHNAFINE -NDW
Solution of Foam destroying Polymers and Polysiloxanes  
Typical Properties

Density at 20o C in g/cc

Non -Volatile Matter in %

Flash Point o C

Solvents

0.84 -0.90

Above 99%

177.0

Nil

Additional Data

Appearance

Color

Solubility in Water

pH value

Opac Liquid (Hazy)

Pale Yellow

Soluble, Milky Emulsion

7.0  !"#

Recommended Level

KRISHNAFINE -NDW

% additive (As Supplied ) based upon

Total Formulation

0.20 -1.0

Incorporation and Processing Instruction
To achieve full effectiveness, the defoamers should be added prior to the grinding process. If adding during later stage, the available shear forces must be high enough good distribution of the defoamers in order to prevent cratering. The full effects of the defoamer achieve 24 hours after incorporation in the system.